Crystal Structure | - Tetragonal ( 4m) : 9oC < T < 130.5 oC
- a=3.99 A c= 4.04 A
|
Growth Method | Top Seeded Solution Growth |
Melting Point | 1600 oC |
Density | 6.02 g/cm3 |
Dielectric constants | - ea = 3700, ec = 135 (unclamped)
- ea = 2400, e c = 60 (clamped)
|
Index of Refraction | - 515 nm 633 nm 800 nm
- no 2.4921 2.4160 2.3681
- ne 2.4247 2.3630 2.3235
|
Transmission wavelength | 0.45 ~ 6.30 mm |
Electro Optic Coefficients: | rT 13 = 11.7 ?1.9 pm/V rT 33 =112 ?10 pm/V rT 42= 1920 ?180 pm/V |
Reflectivity of SPPC ( at 0 deg. cut ) | - 50 - 70 % ( max. 77% ) for l = 515 nm
- 50 - 80 % ( max: 86.8%) for l = 633 nm
|
Two-wave mixing coupling constant: | 10 -40 cm-1 |
Absorption loss: | - l: 515 nm 633 nm 800 nm
- a: 3.392cm-1 0.268cm-1 0.005cm-1
|