Li - Lithium Metal Foil

Lithium Chip 16 mm Dia x 0.6 mm Thickness for Li-ion Battery R&D - EQ-Lib-LiC60(부가세 별도)

Lithium Chip 16 mm Dia x 0.6 mm Thickness for Li-ion Battery R&D - EQ-Lib-LiC60(부가세 별도)

기본 정보
Product Name Lithium Chip 16 mm Dia x 0.6 mm Thickness for Li-ion Battery R&D - EQ-Lib-LiC60(부가세 별도)
Sale Price 960,000원
Product Code EQ-Lib-LiC60
Quantity 수량증가수량감소
상품 옵션
 

Lithium chip is widely used for Li-ion and Li metal rechargeable battery R&D, Please click the link below to see a paper published in Nature Communication which used MTI's Li metal foil:    


SPECIFICATIONS:

   Purity     •  99.9% Lithium
   Melting Point     •  180.5 °C
   Density     •  0.534 g/cm3
   Color     •  Silver
   Dimension     •  16 mm x 0.6 mm (diameter x thickness)
   Quantity     •  100g/bottle (around 1400 pcs/ bottle)

   Packaging

   

     •  Chips are sealed in hot sealing bag in Argon gas glove box with
         < 1 ppm H2O level

     •  Silica gel desiccant pack is sealed in the bag along with the Li
        chips to ensure dryness during shipping

     •  Shelf Life: ~10 days in air at room temperature after shipping

     •  Please open the aluminum can and check the lithium chips
        through the hot sealing bag for any corrosion upon receiving
        the package.
MTI only guarantee that the lithium chips are in
        good conditions upon receiving the package. Proper handling
        and storage of lithium chips from that point on are buyer's
        responsibility.

     •  Please transfer and store the package inside a glove box with
         Argon gas and moisture less than 2%RH upon receiving the
         package, and use the lithium chips as soon as possible. Do not
         use N2 gas glove box as N2 gas is not inert to lithium

     •  When transferring the package through the glove box antechamber,
        please gradually vacuum the antechamber to ~-0.05 MPa instead
        of the full vacuum to avoid popping the package. Then, gradually
        refill the antechamber with high purity Ar gas back to atmospheric
        pressure. Repeat this purging process 5 - 10 times, and then
        transfer the package into the main chamber

   
   Before Use

     •  Package must be opened inside a glove box with Argon gas and
         moisture  less than 2%RH

     •  Clean the surface of the lithium chip using a nylon brush/stainless
         steel  scalpel until a shiny silvery surface appears
        (inside an Argon glove box)

   
   Shipping Limitations

     •  Shipments of Lithium foil are described as “UN 1415, Lithium, 4.3,
         PG I"
.  
     •  All shipments are Hazard Class 4.3 and require “Dangerous when
        wet”
  labels.
     •  Sea Class 4.3 (IMDG)

     •  Road, Rail Class 4.3 11a (RID/ADR)

 
   Safety Data Sheet

             


   Application Notes

   

     •  MTI only sells Li chips within the USA and does not accept
        international order due to restrictions on hazard material
        exportation!!!

     •  MTI reserves the right to charge additional handling fee due to
        special  shipping/handling requirement

     •  Operation and Storage: Lithium is very active in the air, as the
            water vapor catalyzes the reaction with nitrogen, oxygen, etc.
            Lithium reacts  violently with liquid water. Please read the SDS
            carefully before handling Lithium chips

     •  Lithium chip has a passivation layer on surface. From our
            customer's  experience, removing the passivation layer will
            increase battery capacity

     •  Clean the surface of the Li chip using a nylon brush/stainless
            steel scalpel until a shiny silvery surface appears (inside an
             Argon glovebox)

     •  If the Li metal is stored in mineral oil, please refer to this guide on
      How to clean mineral oil off Lithium metal using anhydrous Toluene

     •  A slight increase of O2 level might be observed in the glove box
        when the package is opened. Please keep circulating the glove
        box with ultra-high purity Ar gas until the required O2 level is
        reached.

 
   Video
         
    Video: How to make solid state battery


     


Lithium Storage Options