SUPER C65 Conductive Carbon Black as Conductive Additive for Lithium-Ion Batteries 70g/ bottle - which is equivalent to P-LI
SPECIFICATIONS
Volatile Content
| 0.15 % max |
Toluene Extract | 0.1% max |
Ash content (600C) | 0.025% max |
Grit content > 45 microns
| <2ppm |
Grit content > 20 microns | 12 ppm |
BET Nitrogen surface area | 62m2/g
|
Adsorption stiffness value | 32ml/5g
|
Moisture | 0.1%
|
Density | 160kg/m3 |
Sulphur Content | 0.02%
|
PH | 10
|
Iron (3) | 2ppm
|
Nickel (3) | 1ppm
|
Vanadium (3) | < 1ppm
|
Chromium (3) | < 1ppm |
Copper (3) | < 1ppm |
CAS Number | 1333-86-4 |
Package | Container Sealed in Al Vacuumed Bag |
Application Notes:
- Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
- Please keep the powder in vacuum box to avoid moisture.
- Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity.
Please click here to download SDS